If you are interested, please contact us: ☎13165362772
About us news forum
Foundry experience

Recommendations for investment materials in dental casting

Model name: Neilynck&Vogt Z4

1. Burnout: Impact heat (rapid shooting or rapid casting)

After setting the bench for at least 30 minutes, the cylinder can also be directly placed in a high-temperature furnace with a maximum temperature of 900C (1.650F) as instructed by the alloy manufacturer (and then the temperature can be raised) for several hours or days after setting. The time for the cylinder to maintain end temperature depends on the size of the cylinder and should be between 30 minutes (3 turns) and 50 minutes (9 turns). If the temperature is below 850C, hold for+15 minutes.

2. Burnout: Normal preheating (overnight)

The holding time at the end temperature is between 30 and 50 minutes, ranging from 0 ° C (0 ° F) to 7 to 9 ° C (40 to 50 ° F) per minute.

Quoted from the N&V website, click here to access the N&V website.

Suggestions for investment materials in jewelry casting

Model name: RANSOM&RANDOLPH Plastic

1.gif

The pouring temperature of the metal will vary slightly depending on the specific alloy used.

The casting temperature of the flask will depend on the type of casting. Please refer to the link for specific temperatures.

QQ:465698496